Re: SolusWax Tips and Tricks

Posted: Wed Jan 23, 2019 5:56 pm
by Kokos
The resin is really thick and goopy is that normal? The Fun to Do resin I got also, is much more "watery".


I have tried alot! Longest exposures I have tried where 30Z on 38sec and 5 sec for normal layers.

Re: SolusWax Tips and Tricks

Posted: Wed Jan 23, 2019 6:06 pm
by Mikkopee
Kokos wrote:The resin is really thick and goopy is that normal? The Fun to Do resin I got also, is much more "watery".


I have tried alot! Longest exposures I have tried where 30Z on 38sec and 5 sec for normal layers.

No its not normal. Its bad. Contact you reseller to replace you SolusWax. I had that same thing. Just stop wasting you time, I spend HOURS trying to solve this and it was bad resin.