by rsaldivar
as far as the white setting of the resin , I use a cheap 10.00 hairdryer , I hold the vat in one hand , then blow med hot air from the bottom , that white film is the wax , it melts and then very easy to mix into the resin without stretching the film after that , I also leave the resin in the vat for days

Re: So what is up with SolusWax Pro?

Posted: Thu Jul 16, 2020 2:18 pm
by rkundla
rsaldivar wrote:as far as the white setting of the resin , I use a cheap 10.00 hairdryer , I hold the vat in one hand , then blow med hot air from the bottom , that white film is the wax , it melts and then very easy to mix into the resin without stretching the film after that , I also leave the resin in the vat for days


Wow, that's a pretty innovative way of doing it. I'd be worried that the heat would stretch the film if I got it too hot.

Re: So what is up with SolusWax Pro?

Posted: Thu Jul 16, 2020 7:42 pm
by M-Williams
Very Cleaver!

Re: So what is up with SolusWax Pro?

Posted: Wed Jul 22, 2020 2:52 pm
by sochin
rsaldivar wrote:I hold the vat in one hand , then blow med hot air from the bottom


Thanks, I might try that if I can`t mix it back in. For now I can usually mix it back in cold in a couple of minutes.

cheers,